SMPTE RP 48 PDF
$30.00
Lubrication of 16- and 8-mm Motion-Picture Prints (R2004)
Published by | Publication Date | Number of Pages | |
SMPTE | 01/01/1999 | 0 |
Description
SMPTE RP 48 – Lubrication of 16- and 8-mm Motion-Picture Prints (R2004)
This practice recognizes that surface treatment of 16- and 8-mm motion-picture prints to reduce the film surface friction coefficient is needed to promote good projection performance. The use of such treatment should result in increased steadiness, reduction of noise in the projector gate, and less tendency toward perforation damage during projection.
Product Details
- Published:
- 01/01/1999
- File Size:
- 1 file , 9.7 KB